Polypropylene Fibre Wave Form
Properties
PP fibre Undee form can be instead of steel fibre in cement concrete for anti-crack. Easy to disperse and construct. USAGE:
1. Suggestion of Additive rate: 5.4kg fibre in one cubic meter concrete. (not less than 2.7kg/M3)
2. Technic of mixture: Put the fibre into detritus first, then put grit to mix for about
2minutes, to make the fibre be dispersed. Then put cement and water to mix as per normal technic
Specification
Raw Material |
Polypropylene |
Fiber Type |
wave form |
Length |
24-60mm |
Fiber Dia. |
0.9±0.1mm |
Melting Point(ºC) |
160-170 |
Acid &Alkali Resistance |
Strong |
Crack Elongation |
15-20% |
Elastic Modulas (MPa) |
5192 |
Tensile Strength(MPa) |
400 min. |
Packaging & Shipping
Packing 1.: 4kgs each PE bag, 12960kgs/1X40`HQ.
Packing 2.: 20kgs each carton, 21600kgs/1X40`HQ
Certifications